Polylactide macroporous biodegradable implants for cell transplantation. II. Preparation of polylactide foams by liquid-liquid phase separation

Макропористые биоразлагаемые имплантаты из полилактида для трансплантации клеток. II. Получение пенополилактида методом жидкость–жидкость фазового разделения
Christian Grandfils, Ph. Teyssié, Véronique Maquet, Ch. Schugens, Robert Jérôme
1996-04-01

freeze-dryingliquid-liquid phase separationmacroporous cell-transplantation implantspolylactide foamsspinodal decomposition
Potential of thermally induced phase separation as a porogen technique has been studied in an effort to produce a surgical implant suitable for cell transplantation. Emphasis has been placed on the liquid-liquid phase separation of solutions of amorphous poly DL-lactide and semicrystalline poly L-lactide in an 87/13 dioxane/water mixture. The related temperature/composition phase diagrams have been set up by turbidimetry, and the possible occurrence of a gel has been discussed. Freeze-drying of some phase-separated polylactide solutions can produce flexible and tough foams with an isotropic morphology. Interconnected pores of 1-10 microns in diameter are expected to result from the spinodal decomposition of the polylactide solutions with formation of co-continuous phases. Thermodynamics of the polymer/solvent pair has a decisive effect on the final macroporous foams, as shown by the dependence of their porosity, density, porous morphology, and mechanical behavior on molecular weight and crystallinity of polylactide and concentration of the original solutions. On the basis of the foam characteristics, potential of the liquid-liquid phase separation (spinodal decomposition) has been compared with the solid/liquid phase separation (solvent crystallization) as a porogen technique.
1
Freeze-drying selected phase-separated solutions produced flexible, tough polylactide foams with isotropic morphology.
2
Polymer molecular weight, crystallinity, and initial solution concentration strongly influenced foam porosity, density, morphology, and mechanical behavior; liquid-liquid separation was compared with solvent crystallization as a porogen technique.
3
Spinodal decomposition with co-continuous phases was expected to generate interconnected pores approximately 1–10 microns in diameter.
4
Temperature-composition phase diagrams were established by turbidimetry for amorphous poly DL-lactide and semicrystalline poly L-lactide in an 87/13 dioxane/water mixture.
5
Thermally induced liquid-liquid phase separation was evaluated as a porogen method for producing biodegradable polylactide implants for cell transplantation.

Polylactide foams and solutions formed from amorphous poly DL-lactide and semicrystalline poly L-lactide in an 87/13 dioxane/water mixture

The effects of liquid–liquid phase separation and polylactide molecular weight, crystallinity, and solution concentration on foam porosity, density, morphology, and mechanical behavior

Publication Details
Publication Date
1996-04-01
Journal
Publisher
ISSN
Cited by
314
Access Type
Author Information
Authors
Christian Grandfils
Ph. Teyssié
Véronique Maquet
Ch. Schugens
Robert Jérôme
Explore further
Open the scid.ai AI chat with a ready-made request: it will find papers on a similar topic and help build a literature review.
Find similar papers in the chat →
Make a presentation
100%