On the Improvement of AA2024 Wear Properties through the Deposition of a Cold-Sprayed Titanium Coating

Улучшение износостойкости AA2024 путем нанесения покрытия из титана методом холодного напыления
Antonello Astarita, Felice Rubino, Pierpaolo Carlone, Alessandro Ruggiero, C. Leone, Silvio Genna, Massimiliano Merola, Antonino Squillace
2016-08-11

AA2024 aluminium alloycold gas dynamic spraylaser post-treatmenttitanium coatingtribological properties
This paper deals with the study of the enhancement of the tribological properties of AA2024 through the deposition of a titanium coating. In particular two different coatings were studied: (1) untreated titanium coating; and (2) post-deposition laser-treated titanium coating. Titanium grade 2 powders were deposited onto an aluminium alloy AA2024-T3 sheet through the cold gas dynamic spray process. The selective laser post treatment was carried out by using a 220 W diode laser to further enhance the wear properties of the coating. Tribo-tests were executed to analyse the tribological behaviour of materials in contact with an alternative moving counterpart under a controlled normal load. Four different samples were tested to assess the effectiveness of the treatments: untreated aluminium sheets, titanium grade 2 sheets, as-sprayed titanium powders and the laser-treated coating layer. The results obtained proved the effectiveness of the coating in improving the tribological behaviour of the AA2024. In particular the laser-treated coating showed the best results in terms of both the friction coefficient and mass lost. The laser treatment promotes a change of the wear mechanism, switching from a severe adhesive wear, resulting in galling, to an abrasive wear mechanism.
1
A 220 W diode-laser post-treatment produced the best friction coefficient and lowest mass loss among the tested samples.
2
Cold gas dynamic spraying deposited titanium grade 2 coatings onto AA2024-T3 sheets to enhance their tribological properties.
3
Laser treatment changed the dominant wear mechanism from severe adhesive wear with galling to abrasive wear.
4
Titanium coating deposition improved the wear behavior of AA2024 compared with untreated aluminium sheets.

AA2024-T3 aluminium alloy sheet with cold-sprayed titanium coating, including untreated and post-deposition laser-treated coatings

Tribological and wear behavior of the coated alloy, including friction coefficient, mass loss, and the transition from severe adhesive wear to abrasive wear after laser treatment

Publication Details
Publication Date
2016-08-11
Journal
Publisher
ISSN
Access Type
Author Information
Authors
Antonello Astarita
Felice Rubino
Pierpaolo Carlone
Alessandro Ruggiero
C. Leone
Silvio Genna
Massimiliano Merola
Antonino Squillace
Explore further
Open the scid.ai AI chat with a ready-made request: it will find papers on a similar topic and help build a literature review.
Find similar papers in the chat
Make a presentation
100%