Development of 17-4 PH Stainless Steel for Low-Power Selective Laser Sintering

Разработка нержавеющей стали 17-4 PH для низкомощного селективного лазерного спекания
Jeng‐Ywan Jeng, Mayur Jiyalal Prajapati, Ajeet Kumar, Jung-Ting Tsai, Yu-Deh Chao, Shanshuo Liu, Fulin Chen
2025-01-19

17-4 PH stainless steellow-power laser additive manufacturingmetal-polymer composite powderselective laser sinteringthermal debinding
Selective laser sintering (SLS) is one of the prominent methods of polymer additive manufacturing (AM). A low-power laser source is used to directly melt and sinter polymer material into the desired shape. This study focuses on the utilization of the low-power laser SLS system to successfully manufacture metallic components through the development of a metal–polymer composite material. In this study, 17-4 PH stainless powders are used and mixed with polyoxymethylene (POM) and high-density polyethylene (HDPE) to prepare the composite powder material. The polymeric mixture is removed during the thermal degreasing process and subsequent sintering results in a solid metallic component. Sinterit Lisa with a 5 W, 808 nm laser source is used to fabricate the green part. For the printing parameters of 140 °C, laser power of 35.87 mJ/mm2, and layer thickness of 100 μm, the printed samples achieved a maximum density of 3.61 g/cm3 and a complete shape. After sintering at 1310 °C for 180 min, the tensile strength of the shrunk sample is 605.64 MPa, the hardness is HRC 14.8, the average shrinkage rate is 22%, and the density is 7.57 g/cm3, which can reach 97% of the theoretical density. This process allows the use of a wide range of particle sizes that the usual AM technologies have, making it a low-cost, low-energy-consumption, high-speed AM technology.
1
A metal–polymer composite of 17-4 PH stainless steel powder with POM and HDPE enables metallic component production using a low-power SLS system.
2
Sintered parts exhibited 22% average shrinkage and 7.57 g/cm³ density, corresponding to 97% of the theoretical density.
3
The developed process supports a broad range of powder particle sizes and is presented as a low-cost, low-energy, high-speed alternative for metal additive manufacturing.
4
Thermal degreasing followed by sintering at 1310 °C for 180 minutes yielded parts with 605.64 MPa tensile strength and HRC 14.8 hardness.
5
Using a 5 W, 808 nm laser, optimized parameters of 140 °C, 35.87 mJ/mm² laser energy density, and 100 μm layers produced complete green parts with 3.61 g/cm³ density.

17-4 PH stainless steel metal–polymer composite powder and the metallic components produced from it by low-power selective laser sintering

The manufacturability and resulting density, tensile strength, hardness, and shrinkage of 17-4 PH stainless-steel components produced by low-power selective laser sintering with polymer removal and subsequent sintering

Publication Details
Publication Date
2025-01-19
Journal
Publisher
ISSN
Cited by
2
Access Type
Author Information
Authors
Jeng‐Ywan Jeng
Mayur Jiyalal Prajapati
Ajeet Kumar
Jung-Ting Tsai
Yu-Deh Chao
Shanshuo Liu
Fulin Chen
Explore further
Open the scid.ai AI chat with a ready-made request: it will find papers on a similar topic and help build a literature review.
Find similar papers in the chat →
Make a presentation
100%