Performance of TiAlN multilayer coatings prepared by hybrid multi-arc ion plating and high-power impulse magnetron sputtering
Эксплуатационные характеристики многослойных покрытий TiAlN, полученных гибридным многоэлектродуговым ионным осаждением и высокомощным импульсным магнетронным распылением
2026-05-18
SCID: 54.1/aey9bp27
Discuss with AI
HiPIMSTiAlN multilayer coatingscorrosion resistancehybrid ion platingwear resistance
Figures from the paper
Abstract (AI)
TiAlN coatings with different modulation ratios were prepared on 42CrMo4 steel by hybrid multiarc ion plating and high-power impulse magnetron sputtering (HiPIMS). As the HiPIMS fraction increased, the coating surface showed fewer macroparticle-related defects and the cross-sectional structure became more uniform and compact. XRD analysis indicated that all coatings were mainly composed of face-centered cubic (Ti,Al)N with a weak AlN peak, while a slight shift of the (111) peak and an increase in the (200) reflection suggested a modulation-ratio-dependent evolution in texture and structural state. Among the alternating coatings, the critical load (LC2) increased from 22 to 47 N and the wear rate decreased from 4.95 × 10−4 to 2.60 × 10−4 μm3⋅(N μm)−1 as the modulation ratio increased from 1:0.5 to 1:2. Electrochemical tests showed that the 1:2 coating exhibited the lowest corrosion current density, the highest polarization resistance, and the largest capacitive arc radius, indicating the best overall corrosion resistance among the alternating coatings. Overall, increasing the HiPIMS contribution effectively improved the comprehensive performance of the alternating TiAlN coatings.
Key Findings
1
All coatings primarily contained face-centered cubic (Ti,Al)N with a weak AlN peak, while texture and structural state varied with modulation ratio.
2
For alternating coatings, increasing the modulation ratio from 1:0.5 to 1:2 raised the critical load (LC2) from 22 to 47 N.
3
Increasing the HiPIMS fraction reduced macroparticle-related surface defects and produced more uniform, compact TiAlN cross-sectional structures.
4
The 1:2 coating showed the best corrosion resistance, with the lowest corrosion current density, highest polarization resistance, and largest capacitive arc radius.
5
The wear rate decreased from 4.95 × 10−4 to 2.60 × 10−4 μm3⋅(N μm)−1 as the modulation ratio increased from 1:0.5 to 1:2.
Research Object
Alternating TiAlN multilayer coatings with different modulation ratios deposited on 42CrMo4 steel by hybrid multi-arc ion plating and HiPIMS
Research Subject
The influence of the HiPIMS contribution and modulation ratio on the coatings’ microstructure, phase texture, adhesion, wear, and corrosion performance