Microwave-Assisted Hydrothermal Rapid Synthesis of Ultralong Hydroxyapatite Nanowires Using Adenosine 5′-Triphosphate
Быстрый микроволновой гидротермальный синтез сверхдлинных нанопроволок гидроксиапатита с использованием аденозин-5′-трифосфата
2022-08-07
SCID: 54.1/cavb8a7t
Discuss with AI
HAP nanowire/chitosan scaffoldadenosine 5′-triphosphate (ATP)calcium oleate precursormicrowave hydrothermal synthesisultralong hydroxyapatite nanowires
Figures from the paper
Abstract (AI)
Ultralong hydroxyapatite (HAP) nanowires are promising for various biomedical applications owing to their chemical similarity to the inorganic constituent of bone, high biocompatibility, good flexibility, excellent mechanical properties, etc. However, it is still challenging to control the formation of ultralong HAP nanowires because of the presence of free PO43− ions in the reaction system containing the inorganic phosphate source. In addition, it takes a long period of time (usually tens of hours) for the synthetic process of ultralong HAP nanowires. Herein, for the first time, we have developed an eco-friendly calcium oleate precursor microwave hydrothermal method using biocompatible adenosine 5′-triphosphate (ATP) as a bio-phosphorus source and water as the only solvent for the rapid synthesis of ultralong HAP nanowires. The controllable hydrolysis of ATP can avoid the premature formation of calcium phosphate nuclei and uncontrollable crystal growth. Microwave heating can significantly shorten the synthetic time from tens of hours required by the traditional heating to 1 h, thus achieving high efficiency, energy saving and low cost. The as-prepared ultralong HAP nanowires with high flexibility have lengths of several hundred micrometers and diameters of 10~20 nm, and they usually self-assemble into nanowire bundles along their longitudinal direction. The as-prepared ultralong HAP nanowire/chitosan porous scaffold has excellent bioactivity, good biodegradation and cytocompatibility owing to the bioactive adenosine adsorbed on the surface of ultralong HAP nanowires. It is expected that ultralong HAP nanowires will be promising for various applications in the biomedical fields, such as bone defect repair, skin wound healing, and as a drug nanocarrier.
Key Findings
1
An eco-friendly microwave-assisted hydrothermal method uses calcium oleate, ATP as a biocompatible phosphorus source, and water as the sole solvent to synthesize ultralong HAP nanowires.
2
Controlled ATP hydrolysis prevents premature calcium phosphate nucleation and uncontrolled crystal growth, enabling formation control of ultralong HAP nanowires.
3
Microwave heating reduces synthesis time from tens of hours to 1 hour, improving efficiency while lowering energy consumption and cost.
4
The synthesized HAP nanowires are highly flexible, several hundred micrometers long, 10–20 nm in diameter, and commonly self-assemble into longitudinal bundles.
5
Ultralong HAP nanowire/chitosan porous scaffolds exhibit excellent bioactivity, biodegradability, and cytocompatibility, partly attributed to adsorbed bioactive adenosine.
Research Object
Ultralong hydroxyapatite (HAP) nanowires synthesized by a calcium oleate precursor microwave-assisted hydrothermal process using adenosine 5′-triphosphate (ATP)
Research Subject
Rapid and controllable formation of ultralong HAP nanowires, including their morphology, flexibility, and the bioactivity, biodegradation, and cytocompatibility of the resulting HAP nanowire/chitosan porous scaffold
Publication Details
Publication Date
2022-08-07
Journal
Publisher
ISSN
Cited by
21
Open access PDF
Access Type
Author Information
Download PDF
Subscribe to digest
References available in scid.ai2
Hierarchical Assembly of Monodisperse Hydroxyapatite Nanowires and Construction of High‐Strength Fire‐Resistant Inorganic Paper with High‐Temperature Flexibility2017
Yolk‐Shell Porous Microspheres of Calcium Phosphate Prepared by Using Calcium L ‐Lactate and Adenosine 5′‐Triphosphate Disodium Salt: Application in Protein/Drug Delivery2015