Liquid‐Phase Sintering of Alumina Coated with Magnesium Aluminosilicate Glass
Жидкофазное спекание глинозёма, покрытого алюмосиликатным стеклом магния
1998-05-01
SCID: 54.1/cvurxjkc
Discuss with AI
aluminaglass basicityliquid-phase sinteringmagnesium aluminosilicate glassspinel and mullite crystallization
Figures from the paper
Abstract (AI)
Densification of alumina coated with a MgO‐Al 2 O 3 ‐SiO 2 (MAS) glass was investigated from 1400° to 1460°C. Spinel was observed to form at the liquid‐alumina interface, whereas mullite crystallized uniformly in the liquid. Spinel and mullite crystallization kinetics were accelerated by smaller alumina particle size. Mullite and spinel crystallization retarded densification by forming a percolating network. Boron doping suppressed spinel formation, and thus alumina sintered to higher densities at low temperature. The concept of glass basicity is proposed as a useful guide for selecting dopants for low‐temperature sintering.
Key Findings
1
Boron doping suppressed spinel formation, enabling higher alumina densities at low temperature; glass basicity was proposed to guide dopant selection.
2
Liquid-phase densification of MAS-glass-coated alumina was investigated between 1400° and 1460°C.
3
Mullite and spinel formed a percolating network that retarded densification.
4
Smaller alumina particles accelerated both spinel and mullite crystallization kinetics.
5
Spinel formed at the liquid–alumina interface, while mullite crystallized uniformly throughout the liquid phase.
Research Object
Alumina coated with MgO–Al2O3–SiO2 (MAS) glass during liquid-phase sintering
Research Subject
Densification behavior and crystallization kinetics of spinel and mullite, including the effects of alumina particle size and boron doping on low-temperature sintering
Publication Details
Publication Date
1998-05-01
Journal
Publisher
ISSN
Cited by
39