Cost-Effective Treatment of Hemihydrate Phosphogypsum and Phosphorous Slag as Cemented Paste Backfill Material for Underground Mine

Экономически эффективная переработка полугидратного фосфогипса и фосфорного шлака для использования в качестве материала для закладочного массива на подземных рудниках
Qinli Zhang, Yuxian Ke, Chongchun Xiao, Xilong Xue, Kang Qian, Fengjian He, Qing Yu
2019-02-03

cemented paste backfilldynamic leachabilityhemihydrate phosphogypsumphosphorous slagunderground mine
The environmental pollution caused by the discharge of phosphogypsum (PG) and phosphorous slag (PS) is a common issue for all countries. In order to fully utilize hemihydrate PG (HPG) and PS and treat goafs in mines, the HPG and PS were used as cementitious materials for cemented paste backfill (CPB). The physical and chemical properties of HPG and PS were first analyzed, and then, the characteristics of CPB were evaluated through fluidity tests, gas detection, uniaxial compressive strength (UCS) tests, bleeding tests, and scanning electron microscopy (SEM). After this, the underground environmental impact of CPB-based HPG and PS was investigated through a dynamic leachability experiment. The results show that (1) the UCS of CPB increases with the increase of the HPG content and mass fraction, and the addition of 3% quicklime can eliminate CO2, H2S, and SO2 generated from the slurry of CPB-based HPG-PS; (2) the addition of 3% quicklime and 5% cement to the HPG-PS mixtures can offset the strength loss of CPB in the late curing stage; (3) the UCS of the recommended specimen reaches 1.15–3.32 MPa after curing from 7 to 28 days, with their slump values varying from 15 mm to 26 mm, and the bleeding rates between 0.87% and 1.15%, which can meet the technical requirements of mining methods; (4) the UCS of CPB is the result of the cohydration reaction of hemihydrate gypsum (HG) in HPG and active Al2O3 and SiO2 in PS; and (5) the leaching indexes meet Category IV of the Chinese Groundwater Quality Standard (DZ/T 0290-2015). The results of this investigation provide a cost-efficient way for the efficient mining of phosphate resources and the comprehensive utilization of HPG and PS.
1
Adding 3% quicklime and 5% cement compensates for late-stage strength loss in hemihydrate phosphogypsum–phosphorous slag backfill.
2
Backfill strength results from cohydration of hemihydrate gypsum with active Al₂O₃ and SiO₂, while leaching meets Category IV of the Chinese Groundwater Quality Standard.
3
Cemented paste backfill strength increases with hemihydrate phosphogypsum content and mass fraction; 3% quicklime removes CO₂, H₂S, and SO₂ generated by the slurry.
4
Hemihydrate phosphogypsum and phosphorous slag can serve as cementitious materials for cost-effective cemented paste backfill in underground mines.
5
The recommended mixture achieves 1.15–3.32 MPa UCS after 7–28 days, 15–26 mm slump, and 0.87–1.15% bleeding, meeting mining-method requirements.

cemented paste backfill made from hemihydrate phosphogypsum and phosphorous slag for underground mine goaf treatment

the engineering performance, gas-generation mitigation, hydration mechanisms, and underground leaching environmental impact of the hemihydrate phosphogypsum–phosphorous slag backfill

Publication Details
Publication Date
2019-02-03
Journal
Publisher
ISSN
Access Type
Author Information
Authors
Qinli Zhang
Yuxian Ke
Chongchun Xiao
Xilong Xue
Kang Qian
Fengjian He
Qing Yu
Explore further
Open the scid.ai AI chat with a ready-made request: it will find papers on a similar topic and help build a literature review.
Find similar papers in the chat
Make a presentation
100%