A study on the synthesis and mechanical property assessment of calcium zirconate perovskite – mullite composites

Исследование синтеза и оценки механических свойств композитов на основе перовскита цирконата кальция и муллита
Mehmet Akif HAFIZOĞLU, T. Boyraz
2026-06-12

bending strengthcalcium zirconate–mullite compositesmechanical propertiesperovskite ceramicswear resistance
This study investigates the physical, mechanical, microstructure analysis and wear properties of ceramic composites consisting of calcium zirconate, mullite and their mixtures in different proportions. Calcium zirconate, a multifunctional perovskite ceramic with promising applications in structural, catalytic, and biomedical fields, was reinforced with mullite to enhance its wear resistance. While pure calcium zirconate samples exhibited low physical and mechanical properties, the addition of mullite improved these properties generally. Increased mullite content significantly improved hardness, bending strength and wear resistance in all composites, particularly in the composite containing equal weight proportions of calcium zirconate and mullite (50 wt.‐% calcium zirconate – 50 wt.‐% mullite). The hardness of pure calcium zirconate was measured as 122.94 HV 1, whereas it reached 325.53 HV 1 for the composite containing 50 wt.‐% calcium zirconate and 50 wt.‐% mullite, indicating a significant improvement in mechanical performance. Similarly, the bending strength increased from 32.02 MPa to 98.68 MPa, and the wear volume of the composite was reduced by more than threefold compared to that of pure calcium zirconate, demonstrating enhanced tribological properties. The results indicate that mullite addition is an effective strategy for improving the mechanical properties and especially wear resistance of calcium zirconate ceramics.
1
Bending strength rose from 32.02 MPa to 98.68 MPa after forming the 50–50 calcium zirconate–mullite composite.
2
Hardness increased from 122.94 HV 1 for pure calcium zirconate to 325.53 HV 1 in the 50–50 composite.
3
Mullite reinforcement generally improved the physical, mechanical, and wear properties of calcium zirconate ceramic composites.
4
The 50 wt.% calcium zirconate–50 wt.% mullite composite provided particularly strong overall performance, including enhanced hardness, bending strength, and wear resistance.
5
The 50–50 composite exhibited more than a threefold reduction in wear volume compared with pure calcium zirconate, demonstrating substantially improved tribological performance.

Calcium zirconate–mullite ceramic composites with varying proportions of calcium zirconate and mullite

The effects of mullite content on the physical, mechanical, microstructural, hardness, bending-strength, and wear properties of calcium zirconate ceramics

Publication Details
Publication Date
2026-06-12
Journal
Publisher
ISSN
Access Type
Author Information
Authors
Mehmet Akif HAFIZOĞLU
T. Boyraz
Explore further
Open the scid.ai AI chat with a ready-made request: it will find papers on a similar topic and help build a literature review.
Find similar papers in the chat →
Make a presentation
100%