Monitoring of keyhole entrance and molten pool with quality analysis during adjustable ring mode laser welding

Контроль входа в ключевое отверстие и расплавленной ванны с анализом качества при лазерной сварке в регулируемом кольцевом режиме
Radovan Kovacevic, Xiangdong Gao, Fanrong Kong, Lin Wang, Masoud Mohammadpour, Baixuan Yang, Jean-Philippe Lavoie, Klaus Kleine
2020-01-10

adjustable ring mode (ARM) laser weldingconfocal sensorkeyhole entrance areamolten pool widthtopside weld geometric characteristics
The process monitoring of the top side and the evaluation of surface quality were applied in adjustable ring mode (ARM) laser welding of 316 stainless steel by using visual monitoring and confocal sensor technology. Experiments were conducted in different power arrangements of an ARM laser. In this study, the process status was evaluated based on the area of keyhole entrance and the width of the pool. The geometric characteristics of the topside weld were measured by a confocal sensor. The shape of the fusion zone was analyzed based on its cross section. The process mechanism of a different mode of ARM laser welding was investigated by analyzing the process status and geometric characteristics of the surface bead. Experimental results showed that dual-mode laser welding could stabilize the keyhole entrance with a uniform weld surface formation in comparison to the pure ring-mode laser weld. The dual-mode laser also generated a wider molten pool with a wider fusion zone than the pure center laser weld.
1
Dual-mode (center+ring) ARM laser welding stabilizes the keyhole entrance and produces a more uniform weld surface than pure ring-mode welding.
2
Dual-mode ARM laser welding produces a wider molten pool and a wider fusion zone than pure center-mode laser welding.
3
Geometric topside weld characteristics were measured by a confocal sensor and fusion zone shape analyzed from cross sections.
4
Process monitoring of top side and surface quality in ARM laser welding of 316 stainless steel was performed using visual monitoring and a confocal sensor.
5
Process status was quantified by measuring keyhole entrance area and molten pool width.

Adjustable ring mode (ARM) laser welding of 316 stainless steel (including keyhole entrance, molten pool, and topside weld geometry)

Monitoring and analysis of process status and surface quality via keyhole entrance area, molten pool width, fusion zone shape, and topside weld geometric characteristics under different ARM laser power/mode arrangements (including comparison of dual-mode, ring-mode, and center-mode effects)

Publication Details
Publication Date
2020-01-10
Journal
Publisher
ISSN
Access Type
Author Information
Authors
Radovan Kovacevic
Xiangdong Gao
Fanrong Kong
Lin Wang
Masoud Mohammadpour
Baixuan Yang
Jean-Philippe Lavoie
Klaus Kleine
Explore further
Open the scid.ai AI chat with a ready-made request: it will find papers on a similar topic and help build a literature review.
Find similar papers in the chat
Make a presentation
100%