Abstract (AI)
An integrated theoretical/numerical framework is established and validated to study the chemical erosion of refractory-metal (tungsten, rhenium, and molybdenum) nozzle inserts in solid-rocket-motor environments, with a primary focus on tungsten. The formulation takes into account multicomponent thermofluid dynamics in the gas phase, heterogeneous reactions at the surface, energy transport in the solid phase, and nozzle material properties. Typical combustion species of nonmetallized ammonium-perchlorate/hydroxyl-terminated-polybutadiene propellants at practical motor operating conditions are considered. The erosion rates calculated by employing three different sets of chemical kinetics data available in the literature for the tungsten-steam reaction have been compared. The effect of considering either of two different tungsten oxides, WO2 or WO3, as the final product of surface reactions is also investigated. The predicted erosion rates compare well with experimental data. The oxidizing species of H2O proved more detrimental than CO2 in dictating the tungsten nozzle erosion. The material recessionrateiscontrolledbyheterogeneouschemicalkineticsbecausethediffusionlimitisnotreached.Theerosion rate increases with increasing chamber pressure, mainly due to higher convective heat transfer and enhanced heterogeneous surface reactions. The tungsten nozzle erodes much more slowly than graphite, but at a rate comparable with that of rhenium. The molybdenum nozzle exhibits the least erosion for flame temperatures lower than 2860 K. Its low melting temperature (2896 K), however, restricts applications for propellants with high flame temperatures.
Key Findings
1
An integrated theoretical and numerical framework was developed and validated for predicting chemical erosion of refractory-metal rocket-nozzle inserts.
2
Predicted tungsten erosion rates agreed well with experiments across three tungsten–steam kinetic datasets and alternative WO2 versus WO3 products.
3
Tungsten erodes much more slowly than graphite but comparably to rhenium; molybdenum erodes least below 2860 K, while its 2896 K melting point limits high-temperature use.
4
Tungsten erosion increases with chamber pressure because of stronger convective heat transfer and enhanced surface reactions.
5
Water vapor is more damaging than carbon dioxide, and tungsten recession is controlled by heterogeneous surface kinetics rather than diffusion.
Research Object
Refractory-metal nozzle inserts (primarily tungsten, with rhenium and molybdenum) in solid-propellant rocket motors
Research Subject
Chemical erosion and material recession rates governed by heterogeneous surface reactions, oxidizing species, pressure, heat transfer, and temperature