Friction and Wear of Hard Yet Tough TiN Coatings Deposited Using High-Power Impulse Magnetron Sputtering

Трение и износ твердых, но вязких TiN-покрытий, нанесенных методом импульсного магнетронного распыления высокой мощности
Yun‐Fei Xu, Qian Zhou, Yixiang Ou, Feiqiang Li, Changyu Ou, Wenbin Xue, Bin Liao, Qingsong Hua, Jidong Cao, Guanshu Qu
2024-05-10

TiN coatingsabrasive wearfracture toughnessfriction and wearhigh-power impulse magnetron sputtering
The friction and wear response of hard coatings is complex, which largely depends on a good combination of hardness and toughness, and their service life is difficult to predict. Hence, in this work, hard yet tough TiN coatings were deposited using high-power impulse magnetron sputtering at 5–10 kW. With increasing sputtering power, the coatings showed a transition in crystal texture from (200) to (111), along with a refinement in microstructure, leading to an improvement in hardness (H) of 29.8–31.2 GPa and an effective Young’s modulus (E*) of 310–365 GPa. The hard yet tough TiN coatings deposited at 6.5 kW exhibited the highest H/E* and H3/E*2 ratios of 0.097 and 0.29, respectively, as well as the highest fracture toughness of 2.1 MPa·m1/2 and elastic recovery of 42.5%. Accordingly, the coatings possessed an enhanced adhesion and cohesion, in terms of micro-scratch critical load (LC3 = 19.67 N) and HF Rockwell HF1 level. The friction and wear response of hard yet tough TiN coatings under the normal load of 1–10 N were investigated to explore their durability and predict their critical load up to failure. Wear mechanisms changed from oxidative to severe abrasive wear, with load increasing from 1 to 10 N. At 2–5 N, a combination of oxidative and abrasive wear was observed. The coatings maintained their integrity up to the critical load of 9.4 N before failure event, with a maximum wear track depth of 1.8 μm, indicating their durability under the loading conditions.
1
High-power impulse magnetron sputtering produced hard yet tough TiN coatings with hardness of 29.8–31.2 GPa and effective Young’s modulus of 310–365 GPa.
2
Increasing sputtering power transformed the crystal texture from (200) to (111) and refined the coating microstructure.
3
The coatings retained integrity up to a critical failure load of 9.4 N, with a maximum wear-track depth of 1.8 μm, demonstrating durability under the tested loads.
4
The optimized coating showed enhanced adhesion and cohesion, with a micro-scratch critical load of 19.67 N and HF1 Rockwell adhesion level.
5
TiN deposited at 6.5 kW achieved optimal toughness-related properties, including H/E* = 0.097, H³/E*² = 0.29, fracture toughness of 2.1 MPa·m¹ᐟ², and elastic recovery of 42.5%.
6
Wear mechanisms progressed from oxidative wear at low loads to combined oxidative–abrasive wear at 2–5 N and severe abrasive wear at 10 N.

Hard yet tough TiN coatings deposited by high-power impulse magnetron sputtering

The friction, wear mechanisms, mechanical properties, adhesion, cohesion, durability, and failure critical load of the TiN coatings under normal loads of 1–10 N

Publication Details
Publication Date
2024-05-10
Journal
Publisher
ISSN
Cited by
11
Access Type
Author Information
Authors
Yun‐Fei Xu
Qian Zhou
Yixiang Ou
Feiqiang Li
Changyu Ou
Wenbin Xue
Bin Liao
Qingsong Hua
Jidong Cao
Guanshu Qu
Explore further
Open the scid.ai AI chat with a ready-made request: it will find papers on a similar topic and help build a literature review.
Find similar papers in the chat →
Make a presentation
100%