Low‐pressure additive manufacturing of continuous fiber‐reinforced polymer composites

Аддитивное производство полимерных композитов, армированных непрерывными волокнами, при пониженном давлении
Heather O'Connor, Denis Pius Dowling
2019-05-22

carbon, glass, and Kevlar fiberscomputed tomographycontinuous fiber-reinforced polymer compositesinterlaminar shear strengthlow-pressure additive manufacturing
Abstract Continuous fiber‐reinforced polymer composites have found a wide range of applications in the automotive and aerospace industry due to their lightweight properties. Recently the use of additive manufacturing (AM) has been developed for the fabrication of these composites. This study investigates the use of both atmospheric and, for the first time, low‐pressure (1 Pa) processing conditions for the AM of continuous carbon, glass, and Kevlar fiber‐reinforced nylon composites. Differential scanning calorimetry was used to compare the thermal properties of the three types of fiber‐reinforced filament prior to printing. It was found that the melting peak was dependent on filament type, which can be related to the polymer processing conditions used during their fabrication. Based on computed tomography measurements, it was found that the use of low‐pressure printing conditions yielded a reduction in porosity for the carbon, glass, and Kevlar printed composites of 5.7%, 1.0%, and 1.7%, respectively. The mechanical properties of the composites were compared, using a short beam shear test, which assisted in the measurement of interlaminar properties. An increase in interlaminar shear strength of 33%, 22%, and 12% was obtained for the carbon, glass, and Kevlar fiber‐reinforced polymer composites, respectively, when printed under low pressure, compared with that obtained at atmospheric pressure.
1
Differential scanning calorimetry showed that the melting peak depends on filament type, likely reflecting differences in polymer processing during filament fabrication.
2
Low-pressure printing reduced porosity by 5.7%, 1.0%, and 1.7% for carbon-, glass-, and Kevlar-reinforced composites, respectively.
3
Low-pressure processing increased interlaminar shear strength by 33% for carbon, 22% for glass, and 12% for Kevlar composites compared with atmospheric printing.
4
The results indicate that low-pressure additive manufacturing can improve porosity and interlaminar mechanical performance in continuous fiber-reinforced nylon composites.
5
The study demonstrates additive manufacturing of continuous carbon, glass, and Kevlar fiber-reinforced nylon composites under both atmospheric and 1 Pa low-pressure conditions.

Continuous carbon-, glass-, and Kevlar-fiber-reinforced nylon composites fabricated by additive manufacturing under atmospheric and low-pressure conditions

The effects of low-pressure (1 Pa) versus atmospheric additive manufacturing on filament thermal behavior, printed-composite porosity, and interlaminar shear strength

Publication Details
Publication Date
2019-05-22
Journal
Publisher
ISSN
Access Type
Author Information
Authors
Heather O'Connor
Denis Pius Dowling
Explore further
Open the scid.ai AI chat with a ready-made request: it will find papers on a similar topic and help build a literature review.
Find similar papers in the chat →
Make a presentation
100%