Synergistic Effects of Maleic Anhydride and Epoxidized Palm Oil on PLA/Tapioca Starch Biocomposites

Синергетическое воздействие малеинового ангидрида и эпоксидированного пальмового масла на биокомпозиты PLA/крахмал тапиоки
Gautheman Kurup, Muhammad Fadzlee Firas Mohd Fadzillah, Nishata Royan Rajendran Royan, Nabilah Afiqah Mohd Radzuan, Abu Bakar Sulong, Farrahshaida Mohd Salleh
2026-01-01

PLA/tapioca starch biocompositesepoxidized palm oil plasticizermaleic anhydride compatibilizerrheological propertiesshort-term food packaging
The proliferation of single‐use plastics (SUPs) has raised concerns about waste management and environmental sustainability. Polylactic acid (PLA) can be used as a green alternative, but its high cost and brittleness have hindered its widespread adoption. This paper explores the use of compatibilizer and plasticizer to enhance the compatibility and flexibility of PLA/tapioca starch (TS) biocomposites. Maleic anhydride (MA) was grafted to form PLA‐g‐MA and used as a compatibilizer followed by the addition of epoxidized palm oil (EPO) as a plasticizer. Results demonstrated an overall positive impact, indicating the opportunity to develop an optimized blend composition. Fourier transform infrared (FTIR) confirmed the presence of new functional groups, while thermal analysis indicated successful compatibilization. Plasticization was verified by a reduced T g . Rheology confirmed pseudoplastic behavior with n value of 0.510 < n < 0.552 and activation energy ( E a ) of 25.25 kJ/mol. Tensile tests showed that the addition of 5% PLA‐g‐MA improved the tensile strength by 13%, while the addition of 2% of EPO doubled the elongation at break. The Young’s modulus of the plasticized blend observed a decrease, which indicated improved ductility. Morphology confirmed compatibilization and demonstrated microfibrils. Overall, the PLA/tapioca biocomposite exhibited favorable properties, high quality, and cost‐effectiveness, indicating good potential in short‐term food packaging applications.
1
Adding 5% PLA-g-MA increased tensile strength by 13%, while adding 2% epoxidized palm oil doubled elongation at break.
2
Epoxidized palm oil reduced the glass-transition temperature and Young’s modulus, indicating enhanced plasticization and ductility.
3
FTIR, thermal analysis, and morphology confirmed successful compatibilization, including new functional groups and microfibril formation.
4
Maleic anhydride grafting produced PLA-g-MA, which improved compatibility between PLA and tapioca starch in the biocomposites.
5
The blends exhibited pseudoplastic rheology, with flow behavior indices of 0.510–0.552 and activation energy of 25.25 kJ/mol, supporting potential use in short-term food packaging.

PLA/tapioca starch biocomposites modified with maleic anhydride-grafted PLA and epoxidized palm oil

The effects of maleic-anhydride compatibilization and epoxidized-palm-oil plasticization on the compatibility, rheological, thermal, mechanical, morphological, and ductility properties of the biocomposites

Publication Details
Publication Date
2026-01-01
Journal
Publisher
ISSN
Access Type
Author Information
Authors
Gautheman Kurup
Muhammad Fadzlee Firas Mohd Fadzillah
Nishata Royan Rajendran Royan
Nabilah Afiqah Mohd Radzuan
Abu Bakar Sulong
Farrahshaida Mohd Salleh
Explore further
Open the scid.ai AI chat with a ready-made request: it will find papers on a similar topic and help build a literature review.
Find similar papers in the chat →
Make a presentation
100%