Thermal Analysis of Polyamide 6 Composites Filled by Natural Fiber Blend

Термический анализ композитов на основе полиамида 6, наполненных смесью натуральных волокон
Esra Erbas Kiziltas, Han‐Seung Yang, Alper Kızıltaş, Sevda Boran, Ertan Özen, Douglas J. Gardner
2016-04-13

Differential scanning calorimetryDynamic mechanical thermal analysisNatural fiber blendPolyamide 6 compositesThermogravimetric analysis
This study describes changes in the viscoelastic and thermal properties of composites made with various percentages (up to 20 wt.%) of a natural fiber blend (a mixture of flax, kenaf, and hemp fibers) and polyamide 6 (PA 6).According to the differential scanning calorimetry (DSC) analyses, the incorporation of natural fibers produced minor changes in the glass transition (Tg), melting (Tm), and crystallization temperature (Tc) of the PA 6 composites.Because of the reinforcing effect of natural fibers, the storage modulus (E') from dynamic mechanical thermal analysis (DMTA) increased as the natural fiber content increased.The E' values at room temperature and Tg were 3960 MPa and 1800 MPa, respectively, with the incorporation 20 wt.% fiber, which were 68% and 193% higher than the E' value of neat PA 6.As the natural fiber content increased, the thermal stability of the composites decreased, and thermogravimetric analysis (TGA) showed that the onset temperature of rapid thermal degradation decreased from around 440 (neat PA 6) to 420 °C (20 wt.% natural fiber blend).The addition of 20 wt.% single type fibers showed comparable DSC and TG results to the incorporation of 20 wt.% natural fiber blends.
1
Adding up to 20 wt.% flax, kenaf, and hemp fiber blend caused only minor changes in PA 6 glass-transition, melting, and crystallization temperatures.
2
Increasing natural-fiber content reduced thermal stability, lowering rapid-degradation onset from approximately 440 °C for neat PA 6 to 420 °C at 20 wt.% fibers.
3
Natural fibers increased composite storage modulus with increasing content; at 20 wt.%, E' reached 3960 MPa at room temperature and 1800 MPa at Tg.
4
The 20 wt.% fiber composite showed storage moduli 68% higher at room temperature and 193% higher at Tg than neat PA 6.
5
Using 20 wt.% single-type fibers produced DSC and thermogravimetric results comparable to those of the 20 wt.% blended-fiber composite.

Polyamide 6 (PA 6) composites filled with a natural fiber blend of flax, kenaf, and hemp

The effects of natural fiber content and blend composition on the composites’ viscoelastic properties, thermal transitions, reinforcement, and thermal stability

Publication Details
Publication Date
2016-04-13
Journal
Publisher
ISSN
Access Type
Author Information
Authors
Esra Erbas Kiziltas
Han‐Seung Yang
Alper Kızıltaş
Sevda Boran
Ertan Özen
Douglas J. Gardner
Explore further
Open the scid.ai AI chat with a ready-made request: it will find papers on a similar topic and help build a literature review.
Find similar papers in the chat →
Make a presentation
100%