Effects of LiCl on crystallization, thermal, and mechanical properties of polyamide 6/wood fiber composites

Влияние LiCl на кристаллизацию, термические и механические свойства композитов на основе полиамида 6 и древесного волокна
Shihua Xu, Lichao Sun, Jun He, Huan Na Han, Haigang Wang, Yiqun Fang, Qingwen Wang
2017-07-31

flexural strengthlithium chloride modificationmelting point reductionnon-isothermal crystallizationpolyamide 6/wood fiber composites
In the presented study, lithium chloride (LiCl) was used as a modifier to reduce the melting point of polyamide 6 (PA6) and low melting point PA6/wood fiber composites (LPA6/WFC) were prepared with a hot‐press machine. Non‐isothermal crystallization analysis revealed that as little as 3 wt% LiCl decreased the crystallinity of LPA6/WFC from 21.43% to approximately 10% and reduced the melting point of composites from above 220°C to below 200°C, hence the composites can be produced industrially as well as severe degradation of wood fibers can be avoided. Both LiCl and wood fibers increased the glass transition temperature (Tg) of LPA6/WFC, and the Tg of the composites can reach up to 83.2°C, indicating that composites subjected to high temperature circumstances can still retain good dimensional stability and rigidity. In addition, the composites exhibited good mechanical properties, revealed by a flexural strength of the composites of up to 92 MPa. POLYM. COMPOS., 39:E1574–E1580, 2018. © 2017 Society of Plastics Engineers
1
A 3 wt% LiCl addition lowered the composite melting point from above 220°C to below 200°C, potentially limiting wood-fiber degradation during processing.
2
Adding only 3 wt% LiCl reduced composite crystallinity from 21.43% to approximately 10%.
3
Both LiCl and wood fibers increased the glass-transition temperature, reaching 83.2°C and indicating improved high-temperature dimensional stability and rigidity.
4
LiCl was introduced as a modifier to lower the melting point of polyamide 6/wood fiber composites for hot-press manufacturing.
5
The composites maintained favorable mechanical performance, with flexural strength reaching up to 92 MPa.

LiCl-modified polyamide 6/wood fiber composites (LPA6/WFC)

The effects of LiCl and wood fibers on the composites’ crystallization, melting point, glass transition temperature, dimensional stability, rigidity, and flexural strength

Publication Details
Publication Date
2017-07-31
Journal
Publisher
ISSN
Access Type
Author Information
Authors
Shihua Xu
Lichao Sun
Jun He
Huan Na Han
Haigang Wang
Yiqun Fang
Qingwen Wang
Explore further
Open the scid.ai AI chat with a ready-made request: it will find papers on a similar topic and help build a literature review.
Find similar papers in the chat →
Make a presentation
100%