Sideways deposition rate and ionized flux fraction in dc and high power impulse magnetron sputtering

Скорость бокового осаждения и доля ионизированного потока при осаждении методом постоянного тока и импульсного магнетронного распыления высокой мощности
Jón Tómas Guðmundsson, Daniel Lundin, Michael A. Raadu, N. Brenning, Hamidreza Hajihoseini, Martin Čada, Zdeněk Hubička, Selen Ünaldi
2020-04-17

HiPIMSdc magnetron sputteringionized flux fractionradial ion depositionsideways deposition rate
The sideways (radial) deposition rate and ionized flux fraction in a high power impulse magnetron sputtering (HiPIMS) discharge are studied and compared to a dc magnetron sputtering (dcMS) discharge, while the magnetic field strength |B| and degree of balancing are varied. A significant deposition of the film forming material perpendicular to the target surface is observed for both sputter techniques. This sideways deposition decreases with increasing axial distance from the target surface. The sideways deposition rate is always the highest in dc operation, while it is lower for HiPIMS operation. The magnetic field strength has a strong influence on the sideways deposition rate in HiPIMS but not in dcMS. Furthermore, in HiPIMS operation, the radial ion deposition rate is always at least as large as the axial ion deposition rate and often around two times higher. Thus, there are a significantly higher number of ions traveling radially in the HiPIMS discharge. A comparison of the total radial as well as axial fluxes across the entire investigated plasma volume between the target and the substrate position allows for revised estimates of radial over axial flux fractions for different magnetic field configurations. It is here found that the relative radial flux of the film forming material is greater in dcMS compared to HiPIMS for almost all cases investigated. It is therefore concluded that the commonly reported reduction of the (axial) deposition rate in HiPIMS compared to dcMS does not seem to be linked with an increase in sideways material transport in HiPIMS.
1
In HiPIMS, radial ion deposition is at least as large as axial ion deposition and often approximately twice as high.
2
Integrated flux estimates show that relative radial film-forming-material flux is generally greater in dcMS than HiPIMS across magnetic-field configurations.
3
Significant sideways deposition perpendicular to the target occurs in both dcMS and HiPIMS, decreasing with increasing axial distance.
4
The reduced axial deposition rate commonly observed in HiPIMS is not attributable to increased sideways material transport compared with dcMS.
5
The sideways deposition rate is consistently higher in dcMS than HiPIMS; magnetic-field strength strongly affects it in HiPIMS but not dcMS.

dc and high power impulse magnetron sputtering discharges

sideways (radial) deposition rate and ionized flux fraction, including their dependence on magnetic field strength, magnetic balancing, discharge mode, and axial distance

Publication Details
Publication Date
2020-04-17
Journal
Publisher
ISSN
Cited by
22
Access Type
Author Information
Authors
Jón Tómas Guðmundsson
Daniel Lundin
Michael A. Raadu
N. Brenning
Hamidreza Hajihoseini
Martin Čada
Zdeněk Hubička
Selen Ünaldi
Explore further
Open the scid.ai AI chat with a ready-made request: it will find papers on a similar topic and help build a literature review.
Find similar papers in the chat →
Make a presentation
100%