Improving the Lifetime of Aluminum-Based Superconducting Qubits through Atomic Layer Etching and Deposition

Увеличение времени жизни сверхпроводящих кубитов на основе алюминия с помощью атомно-слоевого травления и осаждения
Jiansong Gao, Loren J. Swenson, Oskar J. Painter, R. Cosmic, Ignace Jarrige, Guillaume Marcaud, Joaquín Minguzzi, Rachel Resnick, Neha Mahuli, Sandra Díez, Matthew Hunt, Jefferson Rose
2025-11-20

atomic layer depositionatomic layer etchingqubit energy relaxation timesuperconducting qubitstwo-level system absorption
We present a dry surface treatment combining atomic layer etching and deposition (ALE and ALD) to mitigate dielectric loss in fully fabricated superconducting quantum devices formed from aluminum thin films on silicon. The treatment, performed as a final processing step prior to device packaging, starts by conformally removing the native metal oxide and fabrication residues from the exposed surfaces through ALE, before in situ encapsulating the metal surfaces with a thin dielectric layer using ALD. We measure a 2-fold reduction in loss attributed to two-level system (TLS) absorption in treated aluminum-based resonators and planar transmon qubits. Treated transmons with compact capacitor plates and gaps achieve median transmon quality factor ( Q ) and transmon qubit energy relaxation time ( T 1 ) values of 3.69 ± 0.42 × 10 6 and 196 ± 22 μs, respectively. These improvements were found to be sustained over several months. We discuss how the combination of ALE and ALD reverses fabrication-induced surface damage to significantly and durably improve device performance via a reduction of the TLS defect density in the capacitive elements.
1
A dry post-fabrication treatment combining atomic layer etching and deposition reduces dielectric loss in aluminum-based superconducting devices.
2
Atomic layer etching removes native oxide and fabrication residues, while in situ atomic layer deposition encapsulates exposed aluminum surfaces with a thin dielectric layer.
3
The performance improvements persist for several months and are attributed to reduced TLS defect density in capacitive elements.
4
The treatment produces a 2-fold reduction in two-level-system absorption loss in aluminum resonators and planar transmon qubits.
5
Treated compact transmons achieve median quality factors of 3.69 ± 0.42 × 10^6 and energy relaxation times of 196 ± 22 μs.

Fully fabricated aluminum-based superconducting quantum devices, including aluminum thin-film resonators and planar transmon qubits on silicon

The durability of device performance improvements through reduced dielectric loss and two-level-system defect density after combined atomic layer etching and deposition, measured by quality factor and energy relaxation time

Publication Details
Publication Date
2025-11-20
Journal
Publisher
ISSN
Cited by
15
Access Type
Author Information
Authors
Jiansong Gao
Loren J. Swenson
Oskar J. Painter
R. Cosmic
Ignace Jarrige
Guillaume Marcaud
Joaquín Minguzzi
Rachel Resnick
Neha Mahuli
Sandra Díez
Matthew Hunt
Jefferson Rose
Explore further
Open the scid.ai AI chat with a ready-made request: it will find papers on a similar topic and help build a literature review.
Find similar papers in the chat →
Make a presentation
100%