Mechanical Properties and Bond Strength of Additively Manufactured and Milled Dental Zirconia: A Pilot Study

Механические свойства и прочность соединения аддитивно изготовленного и фрезерованного стоматологического циркония: пилотное исследование
Simel Ayyıldız, Nurten Baysal, Ülkü Tuğba Kalyoncuoğlu
2021-12-23

Vickers hardness (Vh)additively manufactured zirconiabond strengthdental ceramicflexural strength (FS)in vitro studymechanical propertiesmilled zirconiapilot study
PURPOSE: To evaluate and compare the mechanical properties and ceramic bond of additively manufactured and milled dental zirconia materials. MATERIALS AND METHODS: 4 × 1. 2 mm) shaped milled (M group) (Nacera Pearl; Doceram) and additively manufactured (AM group) (NanoParticle Jetting; XJet, Carmel 1400) zirconia specimens were prepared for 2 experimental groups. Ceramic was applied to the disc specimens (h = 4 mm, r = 6 mm) (n = 9) and their shear bond strength (SBS) was measured. The surface morphology of disc specimens was analyzed with a scanning electron microscope (SEM). The Vickers microhardness (Vh), surface roughness (Ra), and three-point flexural strength (FS) of bar specimens (n = 9) were measured. Results were statistically analyzed with Mann-Whitney U-test (α = 0.05). RESULTS: Significant differences were found in FS and Vh values of the M and AM groups. M group (1501.4 ± 60.1 HV1) showed a significantly higher Vh value than the AM group (1169.2 ± 48.4 HV1) (p < 0.001). FS of the M group (1287.5 ± 115.2 MPa) exhibited significantly high value than the AM (1030.0 ± 29.2 Mpa) group (p < 0.001). Statistically, no significant differences were seen in SBS and Ra values of the M and AM groups. CONCLUSION: Within the limitations of this in vitro study, the manufacturing technique affected the mechanical properties of the zirconia materials. AM zirconia material showed lower Vh and FS values than M zirconia. Additionally AM zirconia demonstrated adequate bond strength with dental ceramic.
1
Additively manufactured (AM) zirconia demonstrated adequate bond strength with dental ceramic despite lower mechanical properties.
2
Additively manufactured (AM) zirconia exhibited lower Vickers hardness (Vh) than milled (M) zirconia.
3
Additively manufactured (AM) zirconia exhibited lower flexural strength (FS) than milled (M) zirconia.
4
Manufacturing technique (additive manufacturing vs milling) affects mechanical properties of dental zirconia in vitro.
5
Study is an in vitro pilot with acknowledged limitations regarding its findings.

Dental zirconia manufactured by additive manufacturing (AM) and by milling (M)

Mechanical properties (Vickers hardness and flexural strength) and bond strength with dental ceramic comparing AM and M zirconia

Publication Details
Publication Date
2021-12-23
Journal
Publisher
ISSN
Cited by
59
Access Type
Author Information
Authors
Simel Ayyıldız
Nurten Baysal
Ülkü Tuğba Kalyoncuoğlu
Explore further
Open the scid.ai AI chat with a ready-made request: it will find papers on a similar topic and help build a literature review.
Find similar papers in the chat →
Make a presentation
100%