Mustafa Bal, Akshay A. Murthy, Shaojiang Zhu, Francesco Crisa, Xinyuan You, Ziwen Huang, Tanay Roy, Jaeyel Lee, D. M. T. van Zanten, Roman Pilipenko, Ivan Nekrashevich, Andrei Lunin, Daniel Bafia, Yu. V. Krasnikova, Cameron Kopas, Ella Lachman, Duncan Miller, J. Mutus, Matthew J. Reagor, Hilal Cansizoglu, Jayss Marshall, David P. Pappas, Kim Vu, Kameshwar K. Yadavalli, Jin‐Su Oh, Lin Zhou, Matthew Joseph Kramer, Florent Lecocq, Dominic P. Goronzy, Carlos G. Torres‐Castanedo, P. Graham Pritchard, Vinayak P. Dravid, James M. Rondinelli, Michael J. Bedzyk, Mark C. Hersam, John Francis Zasadzinski, Jens Koch, James A. Sauls, Alexander Romanenko, Anna Grassellino
2024-04-26

T1 relaxation timeniobium oxidesniobium surface encapsulationsuperconducting qubit coherencetransmon qubits
Abstract We present a transmon qubit fabrication technique that yields systematic improvements in T 1 relaxation times. We encapsulate the surface of niobium and prevent the formation of its lossy surface oxide. By maintaining the same superconducting metal and only varying the surface, this comparative investigation examining different capping materials, such as tantalum, aluminum, titanium nitride, and gold, as well as substrates across different qubit foundries demonstrates the detrimental impact that niobium oxides have on coherence times of superconducting qubits, compared to native oxides of tantalum, aluminum or titanium nitride. Our surface-encapsulated niobium qubit devices exhibit T 1 relaxation times 2–5 times longer than baseline qubit devices with native niobium oxides. When capping niobium with tantalum, we obtain median qubit lifetimes above 300 μs, with maximum values up to 600 μs. Our comparative structural and chemical analysis provides insight into why amorphous niobium oxides may induce higher losses compared to other amorphous oxides.
1
Across capping materials and substrates from different qubit foundries, niobium oxides are more detrimental to coherence than native oxides of tantalum, aluminum, or titanium nitride.
2
Comparative structural and chemical analyses suggest that amorphous niobium oxides produce higher losses than other amorphous oxides.
3
Surface encapsulation of niobium suppresses formation of lossy native niobium oxide and systematically improves transmon T1 relaxation times.
4
Surface-encapsulated niobium qubits achieve T1 relaxation times 2–5 times longer than baseline devices with native niobium oxides.
5
Tantalum-capped niobium devices reach median qubit lifetimes above 300 μs, with maximum values up to 600 μs.

surface-encapsulated niobium transmon qubit devices

T1 relaxation times and coherence losses as a function of niobium surface encapsulation and capping material

Publication Details
Publication Date
2024-04-26
Journal
Publisher
ISSN
Access Type
Author Information
Authors
Mustafa Bal
Akshay A. Murthy
Shaojiang Zhu
Francesco Crisa
Xinyuan You
Ziwen Huang
Tanay Roy
Jaeyel Lee
D. M. T. van Zanten
Roman Pilipenko
Ivan Nekrashevich
Andrei Lunin
Daniel Bafia
Yu. V. Krasnikova
Cameron Kopas
Ella Lachman
Duncan Miller
J. Mutus
Matthew J. Reagor
Hilal Cansizoglu
Jayss Marshall
David P. Pappas
Kim Vu
Kameshwar K. Yadavalli
Jin‐Su Oh
Lin Zhou
Matthew Joseph Kramer
Florent Lecocq
Dominic P. Goronzy
Carlos G. Torres‐Castanedo
P. Graham Pritchard
Vinayak P. Dravid
James M. Rondinelli
Michael J. Bedzyk
Mark C. Hersam
John Francis Zasadzinski
Jens Koch
James A. Sauls
Alexander Romanenko
Anna Grassellino
Explore further
Open the scid.ai AI chat with a ready-made request: it will find papers on a similar topic and help build a literature review.
Find similar papers in the chat →
Make a presentation
100%