Time-resolved measurement of film growth during high-power pulsed magnetron sputtering (HIPIMS) of titanium
Измерение роста плёнки с временным разрешением при высокомощном импульсном магнетронном распылении (HIPIMS) титана
2013-03-22
SCID: 54.1/t9fs2kyb
Discuss with AI
Gas rarefactionHigh-power pulsed magnetron sputteringRotating shutter techniqueTime-resolved growth rateTitanium film growth
Figures from the paper
Abstract (AI)
The growth rate during high-power pulsed magnetron sputtering (HIPIMS) of titanium is measured with a temporal resolution of up to 25 µ s using a rotating shutter concept. According to that concept a 200 µ m slit is rotated in front of the substrate synchronous with the HIPIMS pulses. Thereby, the growth flux is laterally distributed over the substrate. By measuring the resulting deposition profile with profilometry, the temporal variation of the growth flux per pulse is deduced. The time-resolved growth rates are measured for 0.25, 0.5 and 1 Pa with pulse lengths of 50, 200 and 400 µ s for an average power of 100 W. We can clearly identify, the individual phases of a HIPIMS pulse consisting of ignition, current rise, gas rarefaction, plateau/self-sputtering, and afterglow as described in the literature. In addition, the maximum film growth is only reached after gas rarefaction, indicating a dynamic change in local transport properties. After the end of the HIPIMS pulse, the growth rate decays following two time constants of 100 µ s and of ∼ms, respectively. The first is consistent with the decay of the ion flux in the afterglow; the second with a decay of reactive neutrals. The absolute comparison of growth rates indicates that a reduction of the efficiency to 30% for very short pulses is typical for a true HIPIMS plasma.
Key Findings
1
A rotating 200 µm slit synchronized with HIPIMS pulses enables titanium growth-flux measurements with temporal resolution down to 25 µs.
2
Maximum film growth occurs only after gas rarefaction, demonstrating dynamically changing local transport properties during the HIPIMS pulse.
3
Post-pulse growth decays with approximately 100 µs and millisecond time constants, associated respectively with ion-flux and reactive-neutral decay.
4
Time-resolved measurements at 0.25–1 Pa and 50–400 µs pulse lengths resolve ignition, current rise, gas rarefaction, plateau/self-sputtering, and afterglow phases.
5
Very short HIPIMS pulses show a growth-efficiency reduction to about 30%, characteristic of a true HIPIMS plasma.
Research Object
Titanium film growth during high-power pulsed magnetron sputtering (HIPIMS)
Research Subject
Temporal growth-flux dynamics and growth-rate efficiency across HIPIMS pulse phases, pressures, and pulse lengths
Publication Details
Publication Date
2013-03-22
Journal
Publisher
ISSN
Cited by
17
Access Type
Author Information
Download PDF
Subscribe to digest
References available in scid.ai2
Cited by3
Plasma diagnostics for understanding the plasma–surface interaction in HiPIMS discharges: a review2014
Dynamic of the growth flux at the substrate during high-power pulsed magnetron sputtering (HiPIMS) of titanium2013
Neutral gas simulation on the influence of rotating spokes on gas rarefaction in high‐power impulse magnetron sputtering2017